How to Refine Gold by the Acid Method
If you are refining filigree or jewelry, shotting is not necessary. 2. Pour the shot into one or more Pyrex or plastic containers. For every ounce of scrap gold you are going to refine you will need a capacity of 300 milliliter. So, for example, if you are refining 10 ounces, you need a 3,000 milliliter (3 liter or 3 quart) container. 3. Add